What Is Bluing Solution Made Of? [Solved]
A bluing solution is made of potassium nitrite and sodium hydroxide dissolved into water. The solution is heated to approximately 275 °F (135 °C). You should leave the part immersed for 15-30 minutes. Rinse the piece in cold water.